In this study, cobalt nanopowder is fabricated by sonochemical polyol synthesis and magnetic separationmethod. First, sonochemical polyol synthesis is carried out at 220oC for up to 120 minutes in diethylene glycol(C4H10O3). As a result, when sonochemical polyol synthesis is performed for 50 minutes, most of the cobalt precursor(Co(OH)2) is reduced to spherical cobalt nanopowder of approximately 100 nm. In particular, aggregation and growth ofcobalt particles are effectively suppressed as compared to common polyol synthesis. Furthermore, in order to obtainfiner cobalt nanopowder, magnetic separation method using magnetic property of cobalt is introduced at an early reductionstage of sonochemical polyol synthesis when cobalt and cobalt precursor coexist. Finally, spherical cobalt nanopowderhaving an average particle size of 22 nm is successfully separated.
키워드
- 제목
- 수산화코발트의 초음파 폴리올 합성과 자성 선별법을 이용한 코발트 나노 분말의 제조
- 제목 (타언어)
- The Fabrication of Cobalt Nanopowder by Sonochemical Polyol Synthesis of Cobalt Hydroxide and Magnetic Separation Method
- 저자
- 변종민; 최명환; 심창민; 김지영; 김영도
- 발행일
- 2015-02
- 저널명
- 한국분말야금학회지
- 권
- 22
- 호
- 1
- 페이지
- 39 ~ 45