상세 보기
Optimization of Cobalt Loading in Co-CeO2 Catalyst for the High Temperature Water-Gas Shift Reaction
- Lee, Yeol-Lim;
- Jha, Ajay;
- Jang, Won-Jun;
- Shim, Jae-Oh;
- Jeon, Kyung-Won;
- ... Jeon, Byong Hun;
- 외 6명
WEB OF SCIENCE
41SCOPUS
42초록
We varied the cobalt loading (10, 15, 25, 35 wt%) to determine the optimum loading in a Co-CeO2 catalytic system used for the high temperature water-gas shift (WGS) reaction. Severe reaction conditions were used to compare the catalytic performances including a very high gas hourly space velocity (142,663 h(-1)) and a high CO concentration (similar to 38%). Among the prepared catalysts, 15% Co-CeO2 exhibited excellent catalytic activity in the temperature range of 350-550 degrees C without promoting the methanation reaction. In addition, this catalyst showed relatively stable activity for 50 h at 400 degrees C. The outstanding performance of 15% Co-CeO2 catalyst is mainly due to the highest amount of dispersed cobalt atoms on the catalyst surface. Additionally, the WGS activity was affected by the oxygen vacancy concentration.
키워드
- 제목
- Optimization of Cobalt Loading in Co-CeO2 Catalyst for the High Temperature Water-Gas Shift Reaction
- 저자
- Lee, Yeol-Lim; Jha, Ajay; Jang, Won-Jun; Shim, Jae-Oh; Jeon, Kyung-Won; Na, Hyun-Suk; Kim, Hak-Min; Lee, Da-We; Yoo, Seong-Yeun; Jeon, Byong Hun; Bae, Jong Wook; Roh, Hyun-Seog
- 발행일
- 2017-07
- 유형
- Article; Proceedings Paper
- 권
- 60
- 호
- 9-11
- 페이지
- 721 ~ 726