온간성형법으로 제조된 Fe 분말의 성형특성

Compaction Properties of Fe Powder Fabricated by Warm Compaction
  • 김세훈
  • 이영중
  • 이제성
  • 김영도

초록

Various approaches have been proposed to increase the green density. Warm compaction method has been used for the reduction of residual stress, the improvement of magnetic properties and the higher densities. In this work, the effect of warm compaction on green density of Fe powder was investigated. After ball-milling of Fe oxide powder for 30 hours, Fe oxide powder was reduced through the hydrogen reduction process. The pure Fe powder and polymer binder were mixed by 3-D tubular mixer. And then the mixed powder was warm-compacted with various compaction pressure and binder contents. The green density of specimen was added polyvinyl binder was higher than any other specimens.

키워드

Warm CompactionNanostructured Fe PowderPolymer BinderWarm CompactionNanostructured Fe PowderPolymer Binder
제목
온간성형법으로 제조된 Fe 분말의 성형특성
제목 (타언어)
Compaction Properties of Fe Powder Fabricated by Warm Compaction
저자
김세훈이영중이제성김영도
발행일
2007-06
저널명
한국분말야금학회지
14
3
페이지
185 ~ 189