The Ni-rich LiNi0.8Co0.1Mn0.1O2 layered oxide (NCM811) is attracting considerable attention as a high-capacity cathode material for rechargeable Li-ion batteries. However, due to its inherent structural/chemical/electrochemical instability, NCM811 with high Ni content suffers from significant performance degradation upon storage even in ambient atmospheres as well as during charge-discharge cycling. Herein, we demonstrate a simple but effective surface-tuning approach to mitigate storage-induced degradation of NCM811, which is based on the conversion of undesirable Li residues to a protective Li3PO4 nanolayer via phosphate treatment. The accelerated storage stability test shows that phosphate-modified NCM811 exhibits remarkably improved electrochemical performance (capacity, cycle life, and rate capability) over the pristine one after being stored under harsh environmental conditions. A combined analytical study indicates that surface tuning through phosphate treatment enhances the storage stability of NCM811 by eliminating impurity-forming Li residues and producing a Li3PO4 nanolayer that inhibits parasitic reactions at the electrode-electrolyte interface. Furthermore, Li3PO4 provides an effective barrier to H2O and CO2 infiltration into the particle agglomerates, thereby suppressing the loss of particle integrity.

키워드

LiNi0.8CO0.1Mn0.1O2; Surface tuning; Lithium phosphate; Storage stability; Residual lithium; LITHIUM-ION BATTERY; ELECTROCHEMICAL PERFORMANCE; LI; STABILITY; LAYER; PROPERTY; EXPOSURE; OXIDE; AIR
제목
Mitigating storage-induced degradation of Ni-rich LiNi0.8Co0.1Mn0.1O2 cathode material by surface tuning with phosphate
저자
Ryu, Won-Gyue; Shin, Hyun-Seop; Park, Min-Sik; Kim, Hansung; Jung, Kyu-Nam; Lee, Jong-Won
DOI
10.1016/j.ceramint.2019.04.092
발행일
2019-08
유형
정기학술지(Article(Perspective Article포함))
저널명
Ceramics International
권
45
호
11
페이지
13942 ~ 13950