Effect of Ta5+ doping on the thermal physical properties of defective fluorite Y3NbO7 ceramics

Citations

WEB OF SCIENCE

11
Citations

SCOPUS

11

초록

The effects of substituting the B cation in A(3)BO(7) ceramics on their thermal physical properties were investigated by applying a large mass difference. Y-3(Nb1-xTax)O-7 (x = 0, 0.1, 0.2, 0.3, 0.4, and 0.5) ceramics were synthesized, and their structural characteristics were determined. All the fabricated Y-3(Nb1-xTax)O-7 ceramics showed defective fluorite structures and glass-like low thermal conductivity (1.18-2.04 W/m center dot K at 25 degrees C) because of the highly distorted crystal structure and significant mass difference. Substitution with Ta5+ enhanced the sintering resistance, leading to superior thermal-insulating performance via grain boundary scattering. Furthermore, the ceramics exhibited excellent coefficients of thermal expansion, implying the promising applicability of Y-3(Nb1-xTax)O-7 as new thermal barrier materials. The effect of mass difference on the thermomechanical properties of the ceramics was examined, suggesting a simple strategy for engineering the chemical composition of new thermal barrier materials.

키워드

mechanical propertiesoxidesthermal barrier coatingsthermal conductivitythermal expansionBOND-LENGTH DISTRIBUTIONSBARRIER COATINGSPHASE-TRANSFORMATIONSCOMPLEX PEROVSKITESFRACTURE-TOUGHNESSCONDUCTIVITYTRANSITIONEXPANSIONZIRCONATEDISORDER
제목
Effect of Ta5+ doping on the thermal physical properties of defective fluorite Y3NbO7 ceramics
저자
Song, DowonPyeon, Janghyeok유명우Jeon, Hak-BeomOh, Yoon-SukSong, TaeseupPaik, UngyuYang, SeungCheolJung, Yeon-Gil
DOI
10.1111/jace.18135
발행일
2022-02
유형
Article
저널명
Journal of the American Ceramic Society
105
2
페이지
1358 ~ 1366