High capacity Li[Li0.2Ni0.2Mn0.6]O-2 cathode materials via a carbonate co-precipitation method

  • Lee, D. -K.
  • Park, Sangho
  • Amine, Khalil
  • Bang, Hyunjoo
  • Parakash, J.
  • ... Sun, Yang-Kook
Citations

WEB OF SCIENCE

134
Citations

SCOPUS

137

초록

Spherical Li[Li0.2Ni0.2Mn0.6]O-2 has been synthesized by a carbonate co-precipitation method. The Li[Li0.2Ni0.2Mn0.6]O-2 with a phase-pure and well-ordered layered structure was synthesized by heat-treatment of a spherical (Ni0.25Mn0.75)(3)O-4 precursor with (LiOHH2O)-H-.. The average particle size of the Li[Li0.2Ni0.2Mn0.6]O-2 powders was approximately 20 mu m and the size distribution was quite narrow due to the homogeneity of the (Ni0.25Mn0.75)CO3. The Li[Li0.2Ni0.2Mn0.6]O-2 electrode calcined at 900 degrees C delivered an initial discharge capacity of approximately 270 mAh g(-1) in the voltage range of 2.0-4.6 V The differential scanning calorimetry (DSC) results for the Li[Li0.2Ni0.2Mn0.6]O-2 prepared at 900 degrees C showed a major exothermic reaction at 270 degrees C.

키워드

cathode materialcarbonate co-precipitationASIthermal stabilitylithium secondary batteriesSITU X-RAYELECTROCHEMICAL PROPERTIESLITHIUMLI
제목
High capacity Li[Li0.2Ni0.2Mn0.6]O-2 cathode materials via a carbonate co-precipitation method
저자
Lee, D. -K.Park, SanghoAmine, Khalil Bang, HyunjooParakash, J.Sun, Yang-Kook
DOI
10.1016/j.jpowsour.2006.07.064
발행일
2006-11
유형
Article
저널명
Journal of Power Sources
162
2
페이지
1346 ~ 1350