초록

This study investigated the interfacial bond behavior of straight steel fiber in ultra-high-performance concrete (UHPC) containing titanium dioxide (TiO2) as an alternative to silica flour. Experiments were conducted for five replacement ratios (i.e., 0%, 25%, 50%, 75%, and 100%) of TiO2. The results indicated a significant improvement in the bond performance of the steel fiber of UHPC containing TiO2. The best performance was exhibited by the 50% replacement ratio specimen, which showed the highest average bond strength and pullout energy of 7.22 MPa and 447.9 mJ, respectively. Although the benefits of adding TiO2 decreased beyond the replacement ratio of 50%, the 100% replacement ratio specimen demonstrated higher bond strengths and pullout energy than those without TiO2. Thus, TiO2 helps suppress the pullout of steel fiber from UHPC more effectively, which was verified by the presence of severe surface scratches on the steel fiber.

키워드

Ultra-high-performance concreteTitanium dioxideSteel fiberInterfacesSurface abrasionComposite materialsBond strength (materials)Oxide mineralsSilicaSteel fibersTitanium alloysTitanium dioxideUltra-high performance concreteInterfacial bondsPullout energyReplacement ratioSilica flourSurface scratchesTitanium dioxides (TiO2)Ultra high performance concretes (UHPC)
제목
Enhancing fiber-matrix interfacial bond in ultra-high-performance concrete containing titanium dioxide
저자
Choi, Hong-JoonOh, TaekgeunYoo, Doo-Yeol
DOI
10.1016/j.matlet.2020.128547
발행일
2020-12
유형
Article
저널명
Materials Letters
280
페이지
1 ~ 5